LHCI-110 Environmentally Friendly Chrome Mist Inhibitor

 

Appearance

colorless and transparent liquid


Molecular structure

 

Chemcials Name

1H,1H,2H,2H-PERFLUOROOCTANESULFONIC ACID

1-Octanesulfonic acid,3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluoro-

 

Synonym

3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluorooctanesulphonicacid; (1H,1H,2H,2H)-Perfluorooctanesulfonic]; 1-Octanesulfonicacid,3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluoro-; 1H,1H,2H,2H-Perfluorooctanesulfonic acid,32% aqueous solution; 

3,3,4,4,5,5,6,6,7,7,8,8,8-Tridecafluorooctanesulfonicacid; 1H,1H,2H,2H-Perfluorooctanesulphonicacid 98%; 

1H,1H,2H,2H-Perfluorooctanesulphonicacid 98%; 

2-(Perfluorohexyl) ethane-1-sulfonicacid

 

CAS No.: 27619-97-2

Molecular formula: C8H5O3F13S

Molecular weight: 428.1677

EINECS: 248-580-6

Related categories: new energy; intermediates; chromium mist inhibitors; fluorinated surfactants

 

Nature

Density: 1,25g/cm3

Acidity coefficient (pKa): 1.31±0.50 (Predicted)

EPA chemical substance information:

1-OctanChemicalbookesulfonicacid,3,3,4,4,5,5,6,6,7,7,8,8,8-tridecafluoro-(27619-97-2)

 

Use

LHCI-110 environmentally friendly chromium mist inhibitor is an efficient and does not contain the international PFOS series of fluorocarbon surfactants. It has good high temperature resistance, oxidation resistance and electrolytic stability during the production of chromium electroplating. It can effectively reduce the concentration of chromic acid in the electroplating workshop, inhibit the volatilization of acid mist, improve the working environment in the electroplating workshop, and reduce costs.

 

Instructions

Add LHCI-110: 0.1ml-0.4ml to each liter of electrolytic bath solution, and increase the amount appropriately for the first use (try to add 20%-30% more when the coverage is complete for the first time) to make the solvent reach a supersaturated state, which can be consumed in the future The situation is added in batches. )

 

When using, be sure to pay attention to the excessive amount of cylinder opening (or addition amount), for example, after adding the chromium mist inhibitor to the surface of the electroplating tank, continue to add an excessive amount of 30% of the original amount to maintain the chromium mist inhibitor. It is always in an excessive state. As time goes by, the foam gradually consumes slowly, and the surface of the electroplating bath is empty (there is no foam space). At this time, it is necessary to add a chromium mist inhibitor. After the foam is covered, add an additional amount of 30 %, and so on.

Electric Golf Cart