Productos
Buscar
Categoría
Productos electrónicos Belleza / cuidado personal Muebles / materiales de construcción Maquinaria automotriz Accesorios de ropa Grandes almacenes Home Servicios logísticos internacionales
Contacto con proveedores
A: Fu

Pintura impermeable de cemento polimérico js--en

Keywords:

Descripción del producto

Product Description: 

JS polymer cement waterproof coating is a two-component water-based waterproof coating made from high-quality modified polymer emulsion and various additives as the organic liquid material, and special cement along with multiple additives as the inorganic powder material, processed through a scientific formula.


Product Features:

1High coating strength and good elongation;

2Suitable for roller or brush application;

3Environmentally friendly and safe;

4Can be applied on damp substrates with strong adhesion;

5Breathable but not permeable to water.


Specification:

Performance Indicators

Technical Indicator

Typical values

Solid content

≥ 70%

76%

Adhesion Strength (Untreated)

≥ 0.5MPa

1.1MPa

Watertightness (0.3MPa, 30min)

Watertightness

Watertightness

Low Temperature Flexibility

-10℃ No Crack

-10℃ No Crack

Tensile Strength (Untreated)

1.2MPa

1.2MPa


Construction Process:

Subgrade treatment → Detailed additional waterproof layer construction → Large area coating waterproof layer construction → Quality inspection and acceptance → Protective isolation layer construction.


Key Points of Construction:

1The construction temperature should be between 5°C and 35°C. Do not construct in rainy or cloudy weather.

2Subgrade treatment: The subgrade should be flat, solid, clean, free of standing water, floating dust, and oil contamination. Rounded treatments should be applied to corners and pipe roots.

3Coating mixing: Refer to the product quality certificate for the mixing ratio. First, add the liquid material and a small amount of water to the mixing bucket, then slowly add the powder material while mechanically stirring. The mixed coating should be used within 2 hours, and no additional water should be added during the use.

4Detailed additional waterproof layer construction: Apply additional layers to detailed nodes such as corners, pipe roots, and drainage outlets. Apply in 2 to 3 coats, and place reinforcing materials in between to ensure the waterproof coating is fully soaked into the reinforcing layer without wrinkles or lifting.

5Large area coating waterproof layer construction: It is advisable to first apply the coating to vertical surfaces and then to horizontal surfaces. Apply in 2 to 3 coats, waiting for the previous coat to fully dry before applying the next. The application direction should be perpendicular to the previous one.

6Protective isolation layer construction: In humid conditions, the drying speed of the product will slow down. Appropriately extend the drying time, conduct a water retention test after the waterproof layer is completely dry, and proceed with the protective isolation layer construction as per design requirements after acceptance.


Precautions:

1、The construction temperature should be between 5°C and 35°C. Do not construct in rainy or cloudy weather.

2、The coating can be diluted with water, but the amount of water added should not exceed 15% of the liquid material.

3、After mixing the coating according to the specified ratio, use it up within 2 hours. Do not add water again during the use.

4、The coating takes 2 to 3 days to fully dry. In humid environments, the drying time should be appropriately extended.

5、The water retention test can be conducted after the coating is fully dry. After passing the acceptance, proceed with the protective isolation layer construction as per design requirements



Product Application:

Used for waterproofing projects in indoor areas of buildings such as bathrooms, kitchens, balconies, floor levels, and floor heating systems. It can also be used as one of the multiple waterproofing layers in non-exposed roof applications.